ASTM B408 UNS N08811 is a specification that covers nickel-iron-chromium alloy UNS N08811 in the form of hot-worked and cold-worked rod and bar. The material, also known as Alloy 800HT, exhibits excellent corrosion resistance, high-temperature strength, and good mechanical properties. Let's delve into the specifics of ASTM B408 UNS N08811 Rod and Bar:

 

1. ASTM B408 UNS N08811 Rod and Bar Composition:

Nickel (Ni): 30.0 - 35.0%

Iron (Fe): 39.5% min.

Chromium (Cr): 19.0 - 23.0%

Aluminum (Al): 0.15 - 0.60%

Titanium (Ti): 0.15 - 0.60%

Carbon (C): 0.06 - 0.10%

Aluminum + Titanium: 0.85 - 1.20%

 

2. ASTM B408 UNS N08811 Mechanical Properties:

  • Tensile Strength: 75 ksi (min) or 515 MPa (min)
  • Yield Strength (0.2% Offset): 30 ksi (min) or 205 MPa (min)
  • Elongation: 30% (min)

 

3. ASTM B408 Incoloy 800HT Round Bar Specifications:

ASTM B408 / ASME SB 408: Standard Specification for Nickel-Iron-Chromium Alloy Rod and Bar

 

4. 1.4958 Incoloy 800HT material Heat Treatment:

Alloy 800HT (UNS N08811) typically requires annealing between 2100 degree F (1149 degree ) and 1850 degree F (1010 degree ) followed by rapid cooling in water or air.

 

5. Incoloy alloy 800HT Rod And Bar Applications:

  • Chemical and petrochemical processing: Used in equipment handling corrosive chemicals and high-temperature environments.
  • Power generation: Suitable for applications involving high-temperature and high-pressure conditions.
  • Aerospace and gas turbine components: Provides high-temperature strength and corrosion resistance.

 

6. ASTM B408 Incoloy 800HT rod Corrosion Resistance:

ASME SB 408 UNS N08811

 

7. 1.4876 Alloy 800HT Availability:

Our company is a professional and reliable one-stop service manufacturer suppliers exports. We not only provide ASME SB 408 UNS N08811 round bar raw materials, but also provide Incoloy 800ht pipes,

 

 

जांच भेजें

whatsapp

टेलीफोन

ईमेल

जांच